FERRITE POWDER #UHE-9
CHEMICAL COMPOSITION: SrO:6Fe2O3
SPECIFIC GRAVITY: 5.03
PACKAGING: 50 lb Plastic Bags
STRENGTH OF TYPICAL MAGNET:
1.3-1.5 MGO Calendered
1.0-1.1 MGO Extruded
TYPICAL MAGNETIC PROPERTIES :
Br- 2350-2500 Gauss
Hc- 2015-2145 Oe
Hci- 2600-3000 Oe
91.75% Ferrite
8.05% Polyisoprene
0.2% Stearic Acid
PHYSICAL PROPERTIES:
Bulk Density- 45-55 lb/cu ft
Mesh Size- 99.9% less than 325
Moisture Content- Less than 0.1%
Average particle size- 1-1.4 micron
APPLICATIONS: Flexible magnets produced by calendered or extrusion type process used for motor segments, automotive ignitions, proximity switches, latching mechanisms, etc.